Beilstein J. Org. Chem. 2009, 5, No. 58, doi:10.3762/bjoc.5.58
Graphical Abstract
Figure 1: Schematic illustration of the main parts of the setup used in our lab for coaxial electrospinning a...
Figure 2: Polarizing optical microscopy photographs of 8CB-containing composite fibres; (a) SmA phase at room...
Figure 3: Microscopy photographs of characteristic samples when varying the flow rate of the liquid crystal in...
Figure 4: Outer fibre diameters as a function of LC flow rate as determined from 50 measurements by optical m...
Figure 5: DSC thermograms on heating of 8CB as bulk and as inclusion compound in PVP fibres produced with dif...
Figure 6: The liquid crystal core shows a transformation from bubbly to smooth and to bubbly again with incre...
Figure 7: Influence of the applied voltage and the flow rate of the polymer solution on the mean fibre diamet...
Figure 8: a), b): 2D X-ray diffraction pattern of oriented fibres at two perpendicular roll-up directions sch...
Figure 9: X-ray diffraction patterns of PVP fibres without LC (a) and of surface-aligned samples of bulk 8CB ...
Figure 10: Schematic sketch of the arrangement of LC molecules and the smectic layers in an electrospun fibre.